To insure the best quality possible, we have always sawed and dried the lumber ourselves. We start with select and prime grade saw logs. All Polleywood lumber is grade sawn, is first air dried to roughly 20 percent moisture content, and then re-stacked and kiln dried to 6 to 8 percent moisture content.
Our posted Lumber Prices are for lumber is sold in the rough. However, we can custom plane and or straight-line rip to customer specifications. (see Finished Lumber)